Diffraction of light beam on microstructured fiber

Автор: Sotsky Alexandr Borisovich, Belskaya Olga Anatolevna, Sotskaya Luidmila Ivanovna

Журнал: Компьютерная оптика @computer-optics

Рубрика: Дифракционная оптика, оптические технологии

Статья в выпуске: 1 т.38, 2014 года.

Бесплатный доступ

A method based on the Green's theorem and the Graph’s addition theorem is used to construct a solution of 2D problem on lateral diffraction of a light beam on a microstructured fiber. It is shown that the solution can be used for computing the angular distribution of the far field intensity in the case of three-dimensional beam diffraction on a microstructed fiber. Diffraction fields appeared at illumination of microstructured fibers by TE and TM polarized Gaussian beams are analyzed.

Diffraction of light on a microstructured fiber, cylindrical functions, gaussian beam, far field