Tribocontact surface exploration after friction in hexanoic acid solution

Бесплатный доступ

Introduction. The paper considers the evolution of friction coefficient of the pair of copper - steel alloy under friction in a hexanoic acid solution in various concentrations, and antiwear properties of the steel-steel friction pair in an oil-acidic medium. The work objective is to explore the effect of hexanoic acid additives on the tribological characteristics of friction pairs under the friction interaction in waterborne and paraffin-based formulations. Materials and Methods. Tribological studies of a brass-steel friction pair were carried out on the AE-5 end-type friction machine. Antiwear characteristics were explored on a four-ball friction machine (FBW) in accordance with the standard GOST 9490-75. When tested at the FBW, the objective parameters of the lubricity of the oiling compositions were: welding load (Рс); wear spot diameter (Dн), critical load (Рк). Roughness parameters of the servovite film were determined through the optical profilometry; its microgeometry and structure at the nanoscale - through the atomic force microscopy...

Еще

Friction coefficient, selective transfer, servovite film, wear scar, welding load, critical load

Короткий адрес: https://sciup.org/142221971

IDR: 142221971   |   DOI: 10.23947/1992-5980-2019-19-4-366-373

Статья научная