Conducted probes have shown, that in fusible clays intensive condensation ceramic splinter descends in temperature range 950-1050 °С, from the moment of education of a liquid phase, thus hole content decreases up to 8-12%. With temperature rise up to 1150°С quantity of a liquid phase increases up to 45-50% that results in increase of hole content. The most uniform pores are observed in samples from the fusible clays keeping a minimum quantity montmorylonyt.