Fractal analysis of the nanomodified composite microstructure
Автор: Smirnov Vladimir Alexeevich, Korolev Evgenij Valerjevich, Danilov Alexander Maximovich, Kruglova Albina Nikolaevna
Журнал: Нанотехнологии в строительстве: научный интернет-журнал @nanobuild
Статья в выпуске: 5 т.3, 2011 года.
Бесплатный доступ
Method of quantitative analysis of microstructure images is offered. The method is based on binary decomposition of image intensity field. It is shown that the results of binary decomposition can give the criteria similar to fractal dimension. Some results of application of the offered method to the analysis of optical and scanning probe images of composite microstructure are discussed.
Nanomodified composite, fractal dimension, image processing
Короткий адрес: https://sciup.org/14265583
IDR: 14265583 | УДК: 691.175.2,