Research of cutting conditions influence on EP718-ID alloy surface layer microstructure while end milling

Автор: Zhidyaev Alexey Nikolaevich, Nosova Ekaterina Alexandrovna

Журнал: Известия Самарского научного центра Российской академии наук @izvestiya-ssc

Рубрика: Механика и машиностроение

Статья в выпуске: 6-3 т.15, 2013 года.

Бесплатный доступ

Hot-stamped blanks from alloy EP718-ID were machined with end mill. The influence of milling cutting conditions on change of surface layer microstructure researched. It is established that with the increase of depth of the removed layer the processes of return and recrystallization at the surface layer are proceeding by local heating while metal cutting.

High-temperature alloy, milling, cutting width, microstructure, grain size, microhardness, return, recrystallization

Короткий адрес: https://sciup.org/148202611

IDR: 148202611   |   УДК: 621.914