Features of physical-mechanical and high-temperature electric properties of ceramic semicinductor based on SnO 2 with MnO 2 and CuO additive agents

Автор: Dobrosmislov S.S., Kirko V.I., Nagibin G.E., Rezinkina O.A., Popov Z.I.

Журнал: Сибирский аэрокосмический журнал @vestnik-sibsau

Рубрика: Технологические процессы и материалы

Статья в выпуске: 1 (41), 2012 года.

Бесплатный доступ

Ceramic semiconductors based on SnO 2 with MnO 2 and CuO additive agents were synthesized. Synthesis temperature was 1300 and 1400 °С. Physical-mechanical and high-temperature electric properties investigation were performed. It is revealed that increase of synthesis temperature for materials with MnO 2, provides for their better agglomeration. Compositions 96 % SnO 2 - 2 % Sb 2O 3 - 2 % CuO, obtained at 1300 °С, have the best electro-physical properties. Resistance of 94 % SnO 2 - 2 % Sb 2O 3 - 2 % CuO - 2 % MnO 2 in high temperature field is 3 times higher. 96 % SnO 2 - 2 % Sb 2O 3 - 2 % MnO 2 have nonlinear currant-voltage characteristic.

Еще

Conductivity, currant-voltage characteristic, ceramic, tin oxide

Короткий адрес: https://sciup.org/148176736

IDR: 148176736

Статья научная