The influence of the microstructure and phase composition on tribological performances of NiCrBsI laser coatings

Бесплатный доступ

The influence of the microstructure and phase composition on tribological performances of Cr-Ni coatings obtained by gas powder laser cladding has been investigated. The fracture mechanisms of coatings during electrocorundum and silicone carbide abrasive wear process have been stablished. The influence of environment on wear intensity during sliding friction has been demonstrated.

Laser cladding, nicrbsi, microhardness, abrasive wear, sliding wear