Influence of ultradisperse additives on the microstructure and properties of tungsten-cobalt alloys from drilling technics working elements
Автор: Lebedev M.P., Vinokurov G.G., Kychkin A.K., Vasilyeva M.I., Maharova S.N., Sivtseva A.V., Fedorov M.V., Dovgal O.V.
Журнал: Известия Самарского научного центра Российской академии наук @izvestiya-ssc
Рубрика: Машиностроение
Статья в выпуске: 1-2 т.12, 2010 года.
Бесплатный доступ
Are carried out researches of microstructure and mechanical properties of test samples of drilling plates from tungsten-cobalt alloys with ultradisperse additives. It is established, that for the majority of the developed structures density of hard-alloy material not below the level of density of control sample without ultradis-perse additives. Practical saving of tungsten-cobalt alloys microstructure is observed at increase of the mainte-nance of ultradisperse additives from silicon carbide. It is revealed, that the most perspective of developed al-loys is hard-alloy material with ultradisperse silicon carbide with maintenance up to 0,1 % which simultane-ously has high microhardness and homogeneous microstructure.
Tungsten-cobalt alloy, ultradisperse additive, microstructure, drilling technics
Короткий адрес: https://sciup.org/148198957